The invention discloses a hydrating molding process and a
raw material formula of concrete faux marble granite
dry powder. The
raw material formula comprises
ceramic residue, mineral
powder,
cement and
quartz sand; the molding process comprises the following steps: mixing color, agitating materials, storing materials, spraying
powder by virtue of a computer, distributing by virtue of a plurality of pipelines, controlling a
manipulator to adjust a pattern, spraying water at
high pressure for hydrating, vibrating to mold, maintaining with steam, and
polishing a surface. The
raw material formula is on the basis of the
ceramic residue and
cement, and the molding process does not need any high-temperature firing, so that the advantages of low carbon, environmental friendliness and
energy conservation are realized; in addition, a finished product molded through the process is high in
simulation degree, the plate is 10 to 30mm in thickness, or a composite layer on the surface of a concrete faux marble granite
composite plate is 3 to 8mm in thickness; all finished bricks are slightly different, have high sense of wholeness, and also show high naturalness while being applied to a specific scene; moreover, the problem of the current
ceramic industry that a wall
brick or a ceramic
brick can only be molded by firing at a high temperature, which causes large
energy consumption, serious
pollution and treatment on lots of ceramic residues produced by the production of the wall
brick or ceramic brick in the traditional
ceramic industry, can be solved.