The invention relates to a borehole reinforcement shielding agent and a preparation method thereof, and belongs to the technical field of
chemical engineering. The shielding agent comprises, by weight, 40-68 parts of organic
silicon resin, 10-22 parts of
acrylate polymers, 6-22 parts of
epoxy resin, 0.5-1.0 part of nano-blocking agents, 10-18 parts of reactive
silicon oil, 0.1-0.5 part of catalysts, 0.5-1 part of emulsifying agents and 80-100 parts of deionized water. The preparation method includes the steps: sequentially adding organic
silicon resin, the
acrylate polymers, the
epoxy resin, the reactive silicon oil and the deionized water into a reaction kettle, uniformly stirring mixture, and adjusting a pH (potential of
hydrogen) value to reach 7-9; adding the emulsifying agents, stirring mixture for 2 hours, adding the nano-blocking agents, stirring mixture for 3 hours, and heating the mixture to reach the temperature of 80-90 DEG C; adding the catalysts, performing reaction for 5hours at the temperature of 100-120 DEG C, cooling mixture to reach the temperature of 50-60 DEG C, keeping the temperature for 2 hours, and performing cooling and discharging. The method is simple inprocess and low in cost, the prepared borehole reinforcement shielding agent is stable in performance and good in quality, the
compressive strength and the sealing capability of sand rock and mud rock cores can be enhanced, and stability is improved.