Environment-friendly degradable plastic and preparation method thereof
An environmentally friendly technology for degradable plastics, applied in the field of polymer materials, can solve the problems of poor mechanical properties of degradable plastics, and achieve the effect of improving thermal stability and comprehensive improvement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Benefits of technology
Problems solved by technology
Method used
Examples
preparation example Construction
[0022] The invention provides an environment-friendly degradable plastic and a preparation method thereof. The degradable plastic comprises the following components in parts by weight: 55-70 parts of polybutylene adipate terephthalate, polybutylene adipate 10-20 parts of propyl ester, 10-15 parts of modified lignin, 5-6 parts of montmorillonite, 3-4 parts of compatibilizer, 0-1 part of lubricant, 0-1 part of light stabilizer; preferred weight Part ratio: 65 parts of polybutylene adipate terephthalate, 15 parts of polypropylene carbonate, 10 parts of modified lignin, 5 parts of montmorillonite, 3 parts of compatibilizer, 1 part of lubricant, 1 part of light stabilizer, so that the overall performance of degradable plastics is good after being optimized in this way.
[0023] In some embodiments of the present invention, the number average molecular weight Mn of the polybutylene adipate terephthalate is 4.26×10 4 g / mol, polydispersity index 2.41; The number average molecular weig
Embodiment 1
[0037] The raw materials of environment-friendly degradable plastics include the following components in parts by weight:
[0038] 55 parts of polybutylene adipate terephthalate, 20 parts of polypropylene carbonate, 15 parts of modified lignin, 5 parts of montmorillonite, 3 parts of compatibilizer, 1 part of lubricant, 1 part of light stabilizer share.
Embodiment 2
[0040] The raw materials of environment-friendly degradable plastics include the following components in parts by weight:
[0041] 65 parts of polybutylene adipate terephthalate, 15 parts of polypropylene carbonate, 10 parts of modified lignin, 5 parts of montmorillonite, 3 parts of compatibilizer, 1 part of lubricant, 1 part of light stabilizer share.
PUM
Property | Measurement | Unit |
---|---|---|
Number average molecular weight | aaaaa | aaaaa |
Number average molecular weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap